low potassium drug skin carbon steel welding rods E4316(J426)
Product Detailed
Related Categories:Welding Rods
1.all position welding,
2. good mechanical properties,rack resistance,
3. less splashed,
4. Current(AC or DC)
426 carbon steel welding rod
GB E4316 equals AWS E6016
Index
Chemical Composition of Deposited Metal(%) | |||||||||||
C | Mn | Si | Ni | Mo | V | S | P | ||||
≤0.12 | ≤1.25 | ≤0.90 | ≤0.20 | ≤0.30 | ≤0.08 | ≤0.035 | ≤0.040 | ||||
Mechanical Properties of Deposited Metal | |||||||||||
Iterms | Tensile Strength (MPa) | Yield Point (MPa) | Elongation % | Impact Value(J) -30 | |||||||
Standard | ≥420 | ≥330 | ≥22 | ≥27 | |||||||
Typical | 450-530 | ≥330 | 25-33 | 80-180 | |||||||
Sizes, pieces & Recommended Current(AC or DC) | |||||||||||
Diameter (mm) | 2.5 | 3.2 | 4.0 | 5.0 | |||||||
Current(A) | 60-90 | 90-130 | 150-190 | 180-230 | |||||||
Note:
1. The welding rods should be baked around 1 hour s at 350 before use.
2. It is good to remove the rust ,oil stain and water before use.
3. Short arc and narrow welding line.